42CrMo4
EN 10083-3 (1.7225) · Normalized / QT
C 0.38–0.45 · Mn 0.6–0.9 · Cr 0.9–1.2 · Mo 0.15–0.3
Normalized / QT
Ac1
745 °CAc3
790 °CMs
300 °CMf
80 °CHardenability & data governance
High. Jominy (EN 10083-3): HRC ~61 @1.5 mm → ~45 @50 mm from quenched end. Every recommendation stores the material-data version (web-ref-2026-10) used at optimization time.
Material properties
Core model features
Density7.85 g/cm³
Thermal conductivity42 W/m·K
Elastic modulus210 GPa
Specific heat460 J/kg·K
Typical quenchOil / polymer
Hardness target (QT)48–52 HRC
Library records
Search, compare and trace materials (live data-access layer)
| Grade | Standard | Family | Typical quench | Ms | CCT/TTT | Status |
|---|---|---|---|---|---|---|
| 42CrMo4 | EN 10083-3 (1.7225) | Low-alloy Cr-Mo heat-treatable steel | Oil or polymer (water possible for small sections) | 300 °C | Available | Reference |
| 20CrMnTi | GB/T 3077 (A26202) | Case-hardening (carburizing) steel | Oil (carburize 930–950 °C → quench 870 °C oil) | 360 °C | Available | Reference |
| H13 | AISI H13 (1.2344 / 4Cr5MoSiV1) | Hot-work tool steel (air-hardening) | Air / pressurized gas / warm oil (hardening 1000–1050 °C) | 340 °C | Available | Reference |
| 52100 / 100Cr6 / GCr15 | AISI 52100 (1.3505 / GB GCr15) | High-carbon through-hardening bearing steel | Oil (harden 830–870 °C → temper 150–180 °C) | 200 °C | Available | Reference |